Why does nobody warn you that a hot day turns a broom finish into a mess?
I did a driveway pour out in Mesa last June, about 900 square feet, and I waited maybe 15 minutes too long before hitting it with the broom. The sun was beating down and the crete went from nice and workable to fighting me on every pass in what felt like 5 minutes flat. I pulled the broom through and got these ugly torn lines with chunks dragging behind, so I ended up scrambling with a magnesium float to smooth it back out and lost the clean look I wanted. What I figured out after that is to keep a jug of water and a spray bottle close and just wet the surface a touch before each pass instead of trying to rush the whole thing while it sets. I also started checking the temp on my phone before I even order the truck, since anything over 95 out there seems to cook it way faster than I plan for. Learned the hard way that brooming is all about timing and the clock runs a lot quicker in real heat, lol. Anyone got a trick for slowing down the set on a hot pour, or do you just eat the extra help and hustle?