PSA: stop casing in with PVA straight from the bottle and calling it a hinge
Ok so this is a debate I keep having at my local bindery meetup in Lansing. Half the folks there swear by full-strength PVA for the hinge, and the other half water it down or use a mix with methyl cellulose. I've seen 3 books from a new binder come back to me with cracked spines after about 6 months because the glue went on thick and dried stiff. My view is a 70/30 PVA to paste mix flexes way better, but I've only tested it on my own work so pinch of salt. What ratio are you all using, and has anyone actually measured how a hinge holds up after a few years?